Skip to content
Speedymason, thin brick simplified
Menu

Install guide: Cold-formed steel studs, girts or purlins with sheathing

Thin brick over steel studs.

Over steel studs, Speedymason Brick Lath is fastened through the sheathing with stainless or non-corrosive self-tapping screws every 8 inches on center, penetrating the stud flange at least 1/4 inch or three exposed threads. Everything else is the same as a wood frame wall: barrier, a full bed of polymer-modified thin set, corners and control joints.

Fasteners

  • Stainless steel or non-corrosive self-tapping, self-drilling screws, #6 or #8 shank, wafer or pancake head
  • Penetrate the stud flange, girt or purlin at least 1/4 inch, or not less than three exposed threads
  • Every 8 inches on center on the fastener strips

Sheathing and substrate

  • 5/8 inch exterior gypsum, glass-mat or cement board, or 5/8 inch plywood or OSB, per the guide specification
  • 7/16 inch plywood or OSB is the minimum; panels must break on studs

Step by step

The sequence.

  1. 1Install the building wrap, sealer or fluid-applied barrier over the sheathing to code. The dimples on the back of the panel act as a watershed over it.
  2. 2Build a starter panel and set the layout from it. Install with the groove facing down and the tongue fully in the groove.
  3. 3Butt panels end to end with no more than 1/8 inch and no less than a dime width between them, and stagger the seams so no two panels end on the same line.
  4. 4Fasten on the fastener strips every 8 inches on center. Break the butt ends on a stud when the sheathing is thinner than 5/8 inch.
  5. 5Use Speedymason outside corner panels at every exterior corner, screwed through the reinforced angle brackets (12 screws per corner).
  6. 6Mix polymer-modified thin set. Trowel it over the guide legs, which meter the depth, or fully back-butter each brick. The brick can be any thin brick from any maker: extruded, saw cut, concrete or manufactured, or glass and ceramic tile in brick sizes.
  7. 7Angle each brick onto the bed-joint leg and press in from the bottom until thin set squeezes around it.
  8. 8Bag the joints between the bricks with grouting/pointing mortar, let it set to the feel of wet beach sand, and strike. Do not bag with thin set.
  9. 9Clean no sooner than 5 days and no later than 10 days after grouting, with the brick maker's cleaner. Seal with the sealer the brick maker specifies.
Wall section showing mortar locked around Speedymason Brick Lath

Watch for

  • Ask a corrosion specialist about the fastener where dissimilar metals meet
  • Control joints every 15 feet, or as the architect or code calls out
  • Fasteners with at least 800 hours of ASTM B117 salt spray protection meet the guide specification
  • Any thin brick from any maker, 3/8 to 1-1/2 inch thick: extruded, saw cut, concrete or manufactured thin brick, and glass or ceramic tile in brick sizes

The two materials

Polymer-modified thin set
The setting bed the brick is pressed into. Polymer modified, meeting ANSI A118.4 shear bond, ASTM C1714 and ASTM C270 Type S, per the guide specification. Stone Lath and Ultra-Speed take a specialty polymer-modified thin set.
Grouting/pointing mortar
Type S or Type N mortar, bagged into the joints between the bricks after they are set, then struck. Never thin set in the joints, and no joint mortar at all on Ultra-Speed, which is dry stacked.

Products Speedymason has approved are listed in the installation guide.

Questions

Asked on the jobsite.

What screw do I use on steel studs?

A stainless or non-corrosive self-tapping screw with a wafer or pancake head, #6 or #8 shank, long enough to reach three threads past the stud flange.

Does the panel need to break on a stud?

Yes when the sheathing is thinner than 5/8 inch. With 5/8 inch sheathing the butt ends can fall between studs.

Installation guide (PDF) Install videos

Other walls

More install guides.

Next step

A wall that is not on this list?

Send a photo or a section and we will tell you how the panel goes on.